Physical Properties Metric English Comments
Viscosity Measurement 345
345
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 140 cSt
140 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 45 cSt
45 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
22 hrs, 150C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Recommended
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Recommended
Pour Point -67.0 °C
-88.6 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(lin)