Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 748 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 748C (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 748LT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 748S (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 748S-UV (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 749B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 797 (NC346) (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants NC-346 Grease Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8170R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8170U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8172 (829) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8172R (829RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® Y H-VAC 25/9 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® Y L-VAC 25/6 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |
|||
Pour Point | -35.0 °C | -31.0 °F | |
Teknor Apex TruVis Esters™ TNTM TriNonyl Trimellitate |
|||
Pour Point | -35.0 °C | -31.0 °F | |
Teknor Apex TruVis Esters™ TOTM TriOctyl Trimellitate |
|||
Pour Point | -35.0 °C | -31.0 °F | |
Teknor Apex TruVis Esters™ TIDTM Tri-Isodecyl Trimellitate |
|||
Pour Point | -35.0 °C | -31.0 °F | |
ChevronTexaco Cetus® DE 100 Texaco Cetus DE oils deliver value through:Long life — Texaco Cetus DE oils have a low sludge-forming tendency and a high solvency for deposits that help to keep compressor parts clean. Their abili.. |
|||
Pour Point | -35.0 °C | -31.0 °F | |
ChevronTexaco Havoline® SAE 10W-30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
ChevronTexaco Supreme SAE 10W-30 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
ChevronTexaco Supreme SAE 5W-30 Synthetic Blend Motor Oil FeaturesChevron Supreme Synthetic Blend Motor Oil is premium quality automotive engine oil.It is formulated with a combination of synthetic and premium quality conventional base oils and specially s.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
ChevronTexaco Syntholube® ISO 100 Compressor Oil FeaturesChevron Syntholube Compressor Oils are synthetic diester-based, oxidation resistant, compressor oils.ApplicationsChevron Syntholube Compressor Oils are used for portable and stationary rotar.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D97 |
ChevronTexaco Syntholube® ISO 68 Compressor Oil FeaturesChevron Syntholube Compressor Oils are synthetic diester-based, oxidation resistant, compressor oils.ApplicationsChevron Syntholube Compressor Oils are used for portable and stationary rotar.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® 6320 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® FGC 150 Compressor Fluid, Synthetic Food Grade ISO 150 Description: ANDEROL FGC 150 Compressor Fluid is a synthetic hydrocarbon (PAO) based lubricant formulated with special additive packages that provide good thermal and oxidative stability to keep val.. |
|||
Pour Point | -35.0 °C | -31.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |