Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® FXD121R PC (Asia Pacific) Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics LNP KONDUIT OX10324 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound, with through-plane and in-plane thermal conductivity of 3.5 W/(m*K) and 15 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 101 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1130 PC UV-stabilized. Good clarity, heat resistance, property retention and dimensional stability. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | |
Glastic Laminates/Shapes 1461 Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |
|||
UL RTI, Mechanical with Impact | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
UL RTI, Mechanical with Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL746B |
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |