Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 428 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 - 220 °C
255 - 428 °F
Average value: 197 °C Grade Count:10
Overview of materials for PET + PBT Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Deflection Temperature at 0.46 MPa (66 psi) 135 - 220 °C
275 - 428 °F
Average value: 207 °C Grade Count:26
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 0.46 MPa (66 psi) 180 - 220 °C
356 - 428 °F
Average value: 210 °C Grade Count:63
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 0.46 MPa (66 psi) 215 - 220 °C
419 - 428 °F
ASTM D1525, HDT Method B
Loxim 230 12HB Polybutylene Terephthalate
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 207 - 220 °C
405 - 428 °F
Average value: 210 °C Grade Count:5
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Deflection Temperature at 0.46 MPa (66 psi) 154 - 220 °C
310 - 428 °F
Average value: 192 °C Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..