Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 100 - 168 °C | 212 - 334 °F | Average value: 144 °C Grade Count:29 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 149 - 168 °C | 300 - 334 °F | Average value: 157 °C Grade Count:3 |
Overview of materials for Nylon 11 with Graphite Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of .. |