Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 203 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 95.0 °C
198 - 203 °F
after thermal post treatment procedure B; ASTM D648-06
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 95.0 °C
194 - 203 °F
Reliance Industries Polypropylene Random Copolymer
Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries
Deflection Temperature at 0.46 MPa (66 psi) 65.0 - 95.0 °C
149 - 203 °F
Average value: 71.2 °C Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 95.0 °C
194 - 203 °F
C.O.I.M. EXTER S® S 101 Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 101: Medium/high rea..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 95.0 °C
194 - 203 °F
C.O.I.M. EXTER S® S 104 L Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 104 L: Same performa..
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 95.0 °C
194 - 203 °F
C.O.I.M. EXTER S® S 201 Special Laminate
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 201: Polyester resin..
Deflection Temperature at 0.46 MPa (66 psi) 68.0 - 95.0 °C
154 - 203 °F
Average value: 81.7 °C Grade Count:41
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Copyright © lookpolymers.com All Rights Reserved