Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF25 L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 HR L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated and Hydrolysis Resistant TPCI# 9357101Informatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF40 UV L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceAppearan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF43 HS L BK001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF43 L BK001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 7176101Information provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF43 L BKN001 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF43 LE BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant Features: Lubricated and Low ExtractablesAppearance: BlackInformatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF45 L BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackProcessing Method: Injection M.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6/6 GF45 TL10 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: PTFE Lubricant (10%)Features: LubricatedInformation provided by TP Composites.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 CF10 TS15 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(13%) and Silicone Lubricant(2%)Features: Lubricated Appearance: BlackInforma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6/6 GF40 TL10 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat StabilizedInformation p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 259 °C | 499 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |