Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 335 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM)
Information provided by Ravago.
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N2000STL Nylon 6 (DAM)
Information provided by Ravago.
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM)
Information provided by Ravago.
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
ASTM D648
Polymer Resources NY6-IM1 Nylon 6, Impact Modified
Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
ASTM D648
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized
Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
ASTM D648
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
PolyOne Stat-Tech™ NJ-10SS/000 Nylon 12 - 10% Stainless Steel Reinforced  (discontinued **)
Data provided by PolyOne.
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Techmer ES Luriblend® POM CO GF10 TL10 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Techmer ES Luriblend® POM CO GF10 TX15 BK 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionApp..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold..
Deflection Temperature at 0.46 MPa (66 psi) 168 °C
335 °F
Unannealed; ASTM D648
Techmer ES Plastiblend® PA6/ABS 1120 GF15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p..
Copyright © lookpolymers.com All Rights Reserved