Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
Network Polymers NPP 25-0616 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | |
LyondellBasell Lupolen® 3821 D MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | |
LyondellBasell Lupolen® UHM 201 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | |
LyondellBasell Lupolen® UHM 301 MDPE, Ultra-High Molecular Weight For the production of very high abrasion and impact resistant parts with lower slip/stick friction, as well as higher stress crack and chemical resistance. Apart from anticorrosion products, this m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
LyondellBasell Alathon® M4612 High Density Polyethylene ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
LyondellBasell Alathon® M5040 High Density Polyethylene ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648-97 |
Ipiranga Petrochem MB 0434 LS-L MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648-97 |
Ipiranga Petrochem MB 0435 MDPE IPQ employs Spherilene technology from Basell in the production of MDPE. The raw materials, which are supplied by COPESUL, are pre-treated and fed into gas-phase reactors, where medium density polye.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
SK Chemicals SKYPEL P137DW Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C @Thickness 3.20 mm |
142 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy DescriptionFormion® FI 200 is an injection molding grade, non-reinforce Ionomer / Nylon Alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Applicatio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | |
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.1 °C | 142 °F | ASTM D648 |
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.1 °C | 142 °F | ASTM D648 |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | ASTM D648 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 61.0 °C | 142 °F | 90 Minute UV Cure; ASTM D648 |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |