Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
ExxonMobil Escorene® LL-8555 LLDPE, Rotational Molding Pellets
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
ExxonMobil Escorene® LL-8556 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-4 type protection, High flowUses: Consumer items, Toys, Food storage bins |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
NOVA Chemicals Novapol® TR-0242-U MDPE Rotational Molding Resin
(discontinued **) Hexene copolymer, Excellent impact, Excellent ESCRApplications: Large parts, Agricultural storage tanksAdditives: Processing antioxidants, UV stabilizersInformation provided by NOVA Chemicals. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 - 118 °C | 122 - 245 °F | Average value: 95.9 °C Grade Count:65 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Lastane 50 PUR Polyurethane (PUR). Unfilled. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Latigray 47/1-01 CX/45 PP Copolymer Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Latilub 37 B01-02S Bio-Polymer Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-2 |
Borealis Daploy™ WB260HMS Polypropylene Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® ELX 50 HNZ TPA Product description: Grilon ELX 50 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow molding applications. Grilon ELX 50 H NZ has the followi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | Unannealed (0.250 in); ASTM D648 |
Entec Hypel® PELLD5/.935 LLDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ASTM D648 |
Diamond Polymers NPP11-0635 Medium Density Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | <= 50.0 °C | <= 122 °F | |
C.O.I.M. EXTER S® S 901 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 901: General purpose.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-2 |
CENTROPLAST BC NF Organic Thermoplastic, 15% Natural Fiber CENTROPLAST BC NF 15 is made of CO2-neutral, sustainable raw-materials with 15% natural fiber.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | ISO 75-2 |
CENTROPLAST BC Organic Thermoplastic CENTROPLAST BC is made of CO2-neutral, sustainable raw-materials.CENTROPLAST has the characteristics of thermoplastics while being 100% recyclable and completely biodegradable by composting accordin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 50.0 °C | 122 °F | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |