Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 50.0 °C | 113 - 122 °F | ASTM D648-06 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | ISO 75.1 |
Solvay Engineered Polymers DEXFLEX® E756 TPO
(discontinued **) Description: DEXFLEX® E756 thermoplastic olefinic elastomer (TPO) is designed for extruded automotive air-bag covers. This material provides excellent rigidity, durability and low-temperature toug.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 - 54.0 °C | 113 - 129 °F | ASTM D648 |
DSM Somos® 7110 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3020 F LDPE Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3020 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3024 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3025 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3032 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LyondellBasell Lupolen® 3412 D LDPE Telephone cable insulationData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA11 GL8 HS UV Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 3841 nat PA12 Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8350 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 45.0 °C | 113 °F | |
LATI Latistat 48/9900-03 EVA Dissipative product based on Ethyl-Vinyl-Acetate (EVA). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |