Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 124 - 220 °C | 255 - 428 °F | Average value: 197 °C Grade Count:10 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 135 - 220 °C | 275 - 428 °F | Average value: 207 °C Grade Count:26 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 - 220 °C | 356 - 428 °F | Average value: 210 °C Grade Count:63 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 215 - 220 °C | 419 - 428 °F | ASTM D1525, HDT Method B |
Loxim 230 12HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 207 - 220 °C | 405 - 428 °F | Average value: 210 °C Grade Count:5 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 154 - 220 °C | 310 - 428 °F | Average value: 192 °C Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |