Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 129 °C | 167 - 264 °F | Average value: 104 °C Grade Count:60 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 - 129 °C | 250 - 264 °F | |
Addcomp PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 121 - 129 °C | 250 - 264 °F | |
Addcomp PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 11.0 - 129 °C | 51.8 - 264 °F | Average value: 96.3 °C Grade Count:114 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 48.0 - 129 °C | 118 - 264 °F | Average value: 95.3 °C Grade Count:109 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |