Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 113 °C
198 - 235 °F
Average value: 102 °C Grade Count:16
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 0.46 MPa (66 psi) 99.0 - 113 °C
210 - 235 °F
Average value: 106 °C Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Deflection Temperature at 0.46 MPa (66 psi) 105 - 113 °C
221 - 235 °F
Average value: 110 °C Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Deflection Temperature at 0.46 MPa (66 psi) 104 - 113 °C
220 - 235 °F
Average value: 111 °C Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Deflection Temperature at 0.46 MPa (66 psi) 94.4 - 113 °C
202 - 235 °F
Average value: 102 °C Grade Count:8
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved