Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Nylene® 406 Nylon 6, 50% RH Injection molding grade. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded from 406 have bet.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ISO 75-1/-2 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C @Thickness 3.20 mm |
360 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C @Thickness 3.20 mm |
360 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C @Thickness 3.20 mm |
360 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PC GF30 TS15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Com.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N100HSL (COND, 50% RH) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N100HSL (DAM) Nylon 6, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Chase Plastics CP Pryme® N100L (DAM) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Tipco Tipcofil® AM 300 - 15% Mineral Reinforced Nylon-6 Compound, with High Heat Stability 15% Mineral Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
E-Polymers TEKAMID® JN110 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 829L Nylon 6 Basic Nylon 6, low viscosity, lubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 829LF Nylon 6 Basic Nylon 6, low viscosity, lubricated. This is FDA approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 830 Nylon 6 Basic Nylon 6, medium viscosity, unlubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 °C | 360 °F | ASTM D648 |
Ashley Polymers Ashlene® 835 Nylon 6 Basic Nylon 6 high viscosity, for coating and laminating applications, FDA approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 - 224 °C | 360 - 435 °F | Average value: 211 °C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |