Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.83 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BAF52 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 300 °C |
3.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.83 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG11 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG1, NG 12 |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 300 °C |
3.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAK34 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 200 °C |
3.83 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 400 °C |
3.83 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 300 °C |
3.83 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAK14 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.90 µm/m-°C @Temperature 20.0 - 400 °C |
3.83 µin/in-°F @Temperature 68.0 - 752 °F |
|
CeramTec Rubalit® A 1898 Alumina, 98% Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |