Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG1, NG 12
Physical Properties Metric English Comments
Density 2.42 g/cc
0.0874 lb/in³
Thermal Properties Metric English Comments
CTE, linear 6.90 µm/m-°C
<br>@Temperature -30.0 - 70.0 °C
3.83 µin/in-°F
<br>@Temperature -22.0 - 158 °F
7.50 µm/m-°C
<br>@Temperature 20.0 - 300 °C
4.17 µin/in-°F
<br>@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 473 °C
883 °F
Optical Properties Metric English Comments
Refractive Index 1.49
<br>@Wavelength 1014 nm
1.49
<br>@Wavelength 1014 nm
Hg
1.50
<br>@Wavelength 587.6 nm
1.50
<br>@Wavelength 587.6 nm
He
1.51
<br>@Wavelength 404.7 nm
1.51
<br>@Wavelength 404.7 nm
Hg
Transmission, Visible 73 %
<br>@Wavelength 690 - 700 nm
73 %
<br>@Wavelength 690 - 700 nm
Internal transmittance of 79% from 690-700 nm.
IR Transmittance 75 %
<br>@Wavelength 2100 - 2600 nm
75 %
<br>@Wavelength 2100 - 2600 nm
Internal transmittance of 82% from 2300-2600 nm.
UV Transmittance 66 %
<br>@Wavelength 390 nm
66 %
<br>@Wavelength 390 nm
Internal transmittance of 72% at 390 nm.
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3.4
3.4
Alkali Class, AR 2
2
Stain Resistance Class, FR 1
1