Polymer Property : CTE, linear = 3.33 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.00 µm/m-°C

@Temperature 23.0 °C
3.33 µin/in-°F

@Temperature 73.4 °F
MD; ASTM D696
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear 6.00 µm/m-°C

@Temperature 200 °C
3.33 µin/in-°F

@Temperature 392 °F
MD; ASTM D696
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
CTE, linear 6.00 µm/m-°C

@Temperature 300 °C
3.33 µin/in-°F

@Temperature 572 °F
MarkeTech Repton 136 Aluminum Oxide
Brand 136 features: Molding-structural.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the..
CTE, linear 6.00 µm/m-°C

@Temperature 900 °C
3.33 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 314 Mullite
Brand 314 features: Superior hot creep.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the..
CTE, linear 6.00 µm/m-°C

@Temperature 300 °C
3.33 µin/in-°F

@Temperature 572 °F
MarkeTech Repton EXP 36 Cordierite Mullite
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 100 °C
3.33 µin/in-°F

@Temperature 68.0 - 212 °F
H.C. Starck HPM 1701 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 300 °C
3.33 µin/in-°F

@Temperature 68.0 - 572 °F
Schott FG3 Conversion Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include BG34, FG13
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LASF46A Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK14 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott P-LASF47 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
CTE, linear 6.00 µm/m-°C

@Temperature 20.0 - 100 °C
3.33 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat..
CTE, linear 6.00 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.33 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAF21 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.00 µm/m-°C

@Temperature 25.0 - 300 °C
3.33 µin/in-°F

@Temperature 77.0 - 572 °F
CeramTec 771 94% Alumina (Al2O3)
Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America.
CTE, linear 6.00 - 8.00 µm/m-°C

@Temperature 20.0 - 200 °C
3.33 - 4.44 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Frequenta® Steatite
Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be..