| Category | Ceramic , Glass |
| Manufacturer | Schott North America |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott N-LAF21 Glass.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 4.28 g/cc | 0.155 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Knoop Microhardness | 730 | 730 | .1/20 |
| Modulus of Elasticity | 124 GPa | 18000 ksi | |
| Poissons Ratio | 0.295 | 0.295 | |
| Shear Modulus | 48.0 GPa | 6960 ksi | calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 6.00 µm/m-°C <br>@Temperature -30.0 - 70.0 °C |
3.33 µin/in-°F <br>@Temperature -22.0 - 158 °F |
|
| 7.10 µm/m-°C <br>@Temperature 20.0 - 300 °C |
3.94 µin/in-°F <br>@Temperature 68.0 - 572 °F |
||
| Specific Heat Capacity | 0.550 J/g-°C | 0.131 BTU/lb-°F | |
| Thermal Conductivity | 0.830 W/m-K | 5.76 BTU-in/hr-ft²-°F | |
| Transformation Temperature, Tg | 653 °C | 1210 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.788 <br>@Wavelength 587.6 nm |
1.788 <br>@Wavelength 587.6 nm |
n<sub>d</sub> |
| 1.79195 <br>@Wavelength 546.1 nm |
1.79195 <br>@Wavelength 546.1 nm |
n<sub>e</sub> | |
| Transmission, Visible | 88.2 % <br>@Thickness 10.0 mm,<br> Wavelength 380 nm |
88.2 % <br>@Thickness 0.394 in,<br> Wavelength 380 nm |
|
| 95.9 % <br>@Thickness 10.0 mm,<br> Wavelength 405 nm |
95.9 % <br>@Thickness 0.394 in,<br> Wavelength 405 nm |
||
| 98.9 % <br>@Thickness 10.0 mm,<br> Wavelength 460 nm |
98.9 % <br>@Thickness 0.394 in,<br> Wavelength 460 nm |
||
| 99.8 % <br>@Thickness 10.0 mm,<br> Wavelength 580 nm |
99.8 % <br>@Thickness 0.394 in,<br> Wavelength 580 nm |
||
| 99.8 % <br>@Thickness 10.0 mm,<br> Wavelength 700 nm |
99.8 % <br>@Thickness 0.394 in,<br> Wavelength 700 nm |
||
| IR Transmittance | 45.5 % <br>@Thickness 10.0 mm,<br> Wavelength 2500 nm |
45.5 % <br>@Thickness 0.394 in,<br> Wavelength 2500 nm |
|
| 99.2 % <br>@Thickness 10.0 mm,<br> Wavelength 1530 nm |
99.2 % <br>@Thickness 0.394 in,<br> Wavelength 1530 nm |
||
| UV Transmittance | 13 % <br>@Thickness 10.0 mm,<br> Wavelength 334 nm |
13 % <br>@Thickness 0.394 in,<br> Wavelength 334 nm |
|
| 48 % <br>@Thickness 10.0 mm,<br> Wavelength 350 nm |
48 % <br>@Thickness 0.394 in,<br> Wavelength 350 nm |
||
| 74.6 % <br>@Thickness 10.0 mm,<br> Wavelength 365 nm |
74.6 % <br>@Thickness 0.394 in,<br> Wavelength 365 nm |
||
| 80.4 % <br>@Thickness 10.0 mm,<br> Wavelength 370 nm |
80.4 % <br>@Thickness 0.394 in,<br> Wavelength 370 nm |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 51.3 | 51.3 | |
| Alkali Class, AR | 1.0 | 1.0 | |
| Stain Resistance Class, FR | 1.0 | 1.0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| B | 1 | |
| Climatic Resistance Test CR | 1 | |
| HG | 2 | |
| K (10-6mm2/N) | 1.46 | |
| Phosphate Resistance PR | 1.3 | |
| T1013.0 (°C) | 659 | |
| T107.6 (°C) | 729 |