Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.5 µm/m-°C @Temperature 400 °C |
10.3 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 20.0 - 600 °C |
10.3 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 20.0 - 600 °C |
10.3 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Industeel SIRIUS S15 Rare Earth Containing Heat Resistant Steel CLI SIRIUS S15 grade is a fully austenitic stainless steel containing 21 Cr, 1.7 Si, 0.17 N and Rare Earth elements (Cerium, Lanthanum,...etc) which make the alloy particularly well designed for hig.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 0.000 - 316 °C |
10.3 µin/in-°F @Temperature 32.0 - 600 °F |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 25.6 - 649 °C |
10.3 µin/in-°F @Temperature 78.0 - 1200 °F |
|
Carlson Nitronic® 60® Austenitic Stainless Steel General DescriptionNitronic 60 is an anti-galling and wear resistant austenitic stainless steel. It provides a significantly lower cost alternative to combat wear and galling when compared with cob.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 25.0 - 500 °C |
10.3 µin/in-°F @Temperature 77.0 - 932 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |
|||
CTE, linear | 18.5 µm/m-°C @Temperature 25.0 - 500 °C |
10.3 µin/in-°F @Temperature 77.0 - 932 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |