Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 8.30 µm/m-°C @Temperature 40.0 - 100 °C |
4.61 µin/in-°F @Temperature 104 - 212 °F |
ASTM E831 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
CTE, linear, Transverse to Flow | 8.30 µm/m-°C @Temperature 40.0 - 100 °C |
4.61 µin/in-°F @Temperature 104 - 212 °F |
ASTM E831 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
CTE, linear, Transverse to Flow | 8.30 µm/m-°C @Temperature 40.0 - 100 °C |
4.61 µin/in-°F @Temperature 104 - 212 °F |
ASTM E831 |
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
CTE, linear, Transverse to Flow | 8.30 µm/m-°C @Temperature 40.0 - 100 °C |
4.61 µin/in-°F @Temperature 104 - 212 °F |
ASTM E831 |
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |