Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature 20.0 °C |
65.6 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East) LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF MF0049I PP (Europe-Africa-Middle East) LNP* THERMOTUF* MF0049I is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant, Chemically Coupled. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature -30.0 - 30.0 °C |
65.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C | 65.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS BKB085 is a 14% glass reinforced toughened heat stabilized black polyamide 66 resin.Information provided by DuPont Performanc.. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C | 65.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
CTE, linear, Transverse to Flow | 118 µm/m-°C @Temperature 23.0 - 60.0 °C |
65.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |