Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C @Thickness 6.40 mm |
250 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific) Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C @Thickness 6.40 mm |
250 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 121 °C @Thickness 3.20 mm |
250 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl EN130P PPE+PS (Asia Pacific) High heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |