Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 6.40 mm
250 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific)
Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications.
Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 6.40 mm
250 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRILOY Lexan_WR6300 AES+PC+SAN
LNP* Lubriloy* Lexan_WR6300 compound is a wear resistant PC+SAN, with proprietary lubricant, for business equipment applications.
Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 3.20 mm
250 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics Noryl EN130P PPE+PS (Asia Pacific)
High heat, extrusion grade PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.