Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 81.1 °C | 178 °F | ASTM D3418 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Glass Transition Temp, Tg | 81.0 °C | 178 °F | DSC |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Glass Transition Temp, Tg | 81.0 °C | 178 °F | |
Eastman Eastar 6763 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 81.0 - 100 °C | 178 - 212 °F | ASTM D3418 |
BiologiQ EcoStarch GS270 Thermoplastic Starch BiologiQ GS270 is a plasticized thermoplastic starch (TPS) called EcoStarch Resin (ESR). It is suitable for blending with petrochemical or bioresins where biobased content is desired. It Can be us.. |