Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 46.0 °C | 115 °F | |
Lucite International Elvacite ® 2927 Acrylic Resin Lucite International has developed novel polymer chemistry which delivers Elvacite® thermoplastic acrylic resins with controlled molecular architecture and enables the coatings formulator to achi.. |
|||
Glass Transition Temp, Tg | 46.0 °C | 115 °F | |
Lucite International Elvacite ® 4067 Acrylic Resin Elvacite® 4067 is a solid acrylic bead resin that has been designed to give good solubility in white spirit for use in combinations with alkyd resins.Elvacite® 4067 has good compatibility with.. |
|||
Glass Transition Temp, Tg | 46.0 °C | 115 °F | |
Styron DL 2241LA Carboxylated SB Performance Features: High stiffness, high mechanical stabilityApplications: Fiber Binding, Nonwovens and Thermo MoldableEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 46.0 °C | 115 °F | |
Styron DL 8816LA Carboxylated SB Performance Features: Excellent fiber bonding, medium stiff hand, good filler acceptanceApplications: Thermo MoldableEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | >= 46.0 °C | >= 115 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® ED1020 Epoxy Preliminary Product Information SheetMaterial Description: A single component, silver-filled epoxy designed for low power semiconductor LED die attach applications. Its unique features include exce.. |