Styron DL 2241LA Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 2241LA Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Performance Features: High stiffness, high mechanical stabilityApplications: Fiber Binding, Nonwovens and Thermo MoldableEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 46.0 °C
115 °F