Polymer Property : Glass Transition Temp, Tg = 146 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 146 °C
295 °F
DSC
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
Glass Transition Temp, Tg 146 °C
295 °F
DSC
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced
Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex
Glass Transition Temp, Tg 146 °C
295 °F
DSC
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex
Glass Transition Temp, Tg 146 °C
295 °F
DSC
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® 3152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Glass Transition Temp, Tg 146 °C
295 °F
ISO 11357-1/-2
Covestro Makrolon® 3156 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® 3158 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® ET3117 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
Glass Transition Temp, Tg 146 °C
295 °F
10°C/min; ISO 11357-1,-2
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..