Polymer Property : Glass Transition Temp, Tg = -55.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -55.9 °C
-68.6 °F
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Glass Transition Temp, Tg -55.9 °C
-68.6 °F
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company
Glass Transition Temp, Tg -55.9 °C
-68.6 °F
DSC
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
Glass Transition Temp, Tg -55.9 °C
-68.6 °F
DSC
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..