Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | ASTM D3417 |
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding .. |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | |
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to.. |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS 456-202 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | |
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | 10°C/min |
Arkema Group Kynar® FLEX 2750 PVDF
(discontinued **) Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne.. |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | DSC |
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod.. |
|||
Glass Transition Temp, Tg | -34.0 °C | -29.2 °F | Compound |
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR) Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It .. |