Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -33.0 - 120 °C | -27.4 - 248 °F | Average value: 44.7 °C Grade Count:18 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | |
LG Chemical SSBR 2550 High Acrylonitrile Polymer Description: LG SSBR 2550 is a solution styrene butadiene rubber (S-SBR) extended with TDAE oil.Applications: SSBR 2550 is a high vinyl content grade, can be used in tire tread to improve rolling re.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | |
LG Chemical SSBR 2550H High Acrylonitrile Polymer Description: LG SSBR 2550 is a solution styrene butadiene rubber (S-SBR) extended with TDAE oil.Applications: SSBR 2550 is a high vinyl content grade, can be used in tire tread to improve rolling re.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | |
LG Chemical SSBR 3626 High Acrylonitrile Polymer Description: LG SSBR 3626 is a solution styrene butadiene rubber (S-SBR) extended with TDAE oil.Applications: SSBR 3626 is a high styrene and medium vinyl content grade, can be used in tire tread to.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | DSC |
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane Features: Very resilient product with excellent resistance to abrasion and tearing, low temperature flexibility, and resistant to certain chemicals.Uses: Hot melt adhesive, synthetic leather and fab.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | DSC |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | -33.0 °C | -27.4 °F | |
Loctite® 3872 1 component acrylic/urethane UV/Heat Cure Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |