Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2351-85AE elastomer is a polyether hybrid specialty polyurethane elastomer compound which combines excellent resistance to fuels and oils with good hydrolytic stability and high damping.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Mallard Creek Polymers ROVENE® 4305 SBR Latex ROVENE® 4305 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This non-woven and textile binder offers outstanding.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Mallard Creek Polymers ROVENE® 5005 SBR Latex ROVENE® 5005 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This paper saturant offers good water and solvent re.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion Applications: Rovene® 6119 is a low glass transition temperature styrene-acrylic polymer that offers flexibility during movement of the substrate and water resistance. Rovene® 6119 also exhibi.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | |
Mallard Creek Polymers ROVENE® 8305 SBR Emulsion ROVENE® 8305 is a 50% bound styrene, high gel content hot polymerized styrene – butadiene emulsion. Compatibility with commercial tackifier resin emulsions is excellent, as is filler toleran.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | DSC |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | DSC |
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 90AF3 TPU is a 90A aromatic polyether-based thermoplastic polyurethane.Features: High moisture vapor transmission, good physical properties and elasticity, free of organo-tin comp.. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | DSC |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Glass Transition Temp, Tg | -24.0 °C | -11.2 °F | DSC |
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2101-85A offers good low temperature properties, fast cycle time, and good hydrolytic stability. Applications include: seals, gaskets, animal tags, molding applications, ho.. |