Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5610Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5621Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5640Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2123 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent hot tear and compression se.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2120 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for difficult extrusions. .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2182 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Dipolymer for autoclave curing. Used.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FG-5630Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | ASTM D4065 |
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | DSC |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | |
Zeon Chemicals Nipol® 1401LG Nitrile Powder and Crumb Elastomer Nipol 1401LG is a copolymer of butadiene and acrylonitrile of excellent oil resistance. This material is ground and dusted with approximately 2.0% mineral anticake which allows direct addition to mi.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | dynamic; DIN 53 736 |
Hippe PP Polypropylene Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | dynamic; DIN 53 736 |
Hippe PVDF Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol.. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl .. |
|||
Glass Transition Temp, Tg | -18.0 °C | -0.400 °F | TR10 |
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia.. |