Thermal Properties Metric English Comments
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ Dipolymer, 35% Carbon Black Filled  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb.
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5620Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5621Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5623Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5640Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5641Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5660Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series O-ring grades are the c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2110Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Viscosity ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2174 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2179 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2180 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Lower mold shrinkage and excellent co..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FE-5622Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. The FE series grades are Dyneon's cle..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2122 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good flow, release and hot tear for c..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2144 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Higher viscosity version of FC-2123. ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2152 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved hot tear over FC-2176. Sugg..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2176 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Good general purpose grade with good ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2181 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Combines high elongation with excelle..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FG-5630Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2145 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2230 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2261Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
Melt
Covestro Bayblend® T88 GF-10* Polycarbonate + SAN Glass Filled Impact Grade
Developmental productInjection molding grade10 % GFoptimized heat ageing- and UV-stabilityvery good flowtensile modulus = 5100 MPaVicat/B 120 = 134 °CPreprocessingMax. Water content
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
Melt
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled
Injection molding grade10 % glass fiber filledtensile modulus = 3900 MPaVicat/B 120 temperature = 131 °CPreprocessingMax. Water content
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2211 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FC-2260 Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 1.8% Luperco™ 101XL Peroxide, and 2.5 % Triallyl ..
Specific Heat Capacity 1.65 J/g-°C
0.394 BTU/lb-°F
3M Dyneon™ Fluorel™ FG-5690Q Fluoroelastomer VF2 + HFP Dipolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. When compared to other food grade Dia..