Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.220 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.920 J/g-°C
0.220 BTU/lb-°F
ASTM E1461-92
Park Electrochemical Nelco® N4000-29 BC® Buried Capacitance™ Multifunctional Epoxy
The Nelco N4000-29 is a lead-free, low-CTE, high Tg multifunctional epoxy substrate which has been designed for use in standard multilayer PWB designs and today’s toughest, high-performance, lead-f..
Specific Heat Capacity 0.920 J/g-°C
0.220 BTU/lb-°F
Mateck Magnesium Fluoride (MgF2)
Optical crystals
Specific Heat Capacity 0.920 J/g-°C
0.220 BTU/lb-°F
ASTM E1269
CoorsTek AD-85 Alumina (nom. 85% Al2O3)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Specific Heat Capacity 0.920 J/g-°C
0.220 BTU/lb-°F
ASTM E1269
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Specific Heat Capacity 0.920 J/g-°C

@Temperature 100 °C
0.220 BTU/lb-°F

@Temperature 212 °F
Silicone Property; ASTM E1952
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier
Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m..
Specific Heat Capacity 0.920 J/g-°C
0.220 BTU/lb-°F
ASTM E1461-92
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy
The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW..
Copyright © lookpolymers.com All Rights Reserved