Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.858 J/g-°C | 0.205 BTU/lb-°F | |
Mateck Glass (BK7 Schott or analogous) Optical crystals |
|||
Specific Heat Capacity | 0.858 J/g-°C | 0.205 BTU/lb-°F | |
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.857 J/g-°C | 0.205 BTU/lb-°F | |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Specific Heat Capacity | 0.857 J/g-°C | 0.205 BTU/lb-°F | |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Specific Heat Capacity | 0.857 J/g-°C | 0.205 BTU/lb-°F | |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |