Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.800 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Calculated
Rogers Corporation RO3010 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:
Specific Heat Capacity 0.800 - 0.840 J/g-°C
0.191 - 0.201 BTU/lb-°F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.800 - 0.840 J/g-°C
0.191 - 0.201 BTU/lb-°F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.800 - 0.840 J/g-°C
0.191 - 0.201 BTU/lb-°F
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Schott Nextrema® 712-6 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Schott Nextrema® 724-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Schott Nextrema® 724-5 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Schott Nextrema® 724-8 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 20.0 - 100 °C
0.191 BTU/lb-°F

@Temperature 68.0 - 212 °F
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler BB-BLOCK Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler BF-BLOCK Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler LR-1750 Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler M-EXTRA 'E' Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler ROTOL Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler SUPRA Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Sapco 99.7% Aluminum Oxide
Information provided by Sapco.
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Schott N-LAF34 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
Skamol Group Moler SM-65 Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 32.0 - 800 °C
0.191 BTU/lb-°F

@Temperature 89.6 - 1470 °F
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation
Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo..
Specific Heat Capacity 0.800 J/g-°C

@Temperature 32.0 - 800 °C
0.191 BTU/lb-°F

@Temperature 89.6 - 1470 °F
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel
Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivit..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
DINV ENV 821-3
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Specific Heat Capacity 0.800 J/g-°C

@Temperature 100 - 200 °C
0.191 BTU/lb-°F

@Temperature 212 - 392 °F
DINV ENV 821-3
CeramTec Rubalit® 708S Alumina, 96%
Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
ASTM E1269
CoorsTek SC-DSLP (SC-50) Liquid Phase Sintered Silicon Carbide
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..
Copyright © lookpolymers.com All Rights Reserved