Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, 10% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, 40% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 0% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 0% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 10% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 10% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 30% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 30% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 50% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, hot rolled, solution annealed plate, 6.4-12.7 mm (1/2 in.) thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, sheet after 1000 hours at 648°C Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 700 °C |
0.142 BTU/lb-°F @Temperature 1290 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, GMAW deposit weld metal Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, plate, 16000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, plate, 16000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 20% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, 50% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, as cast vacuum investment casting Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 800 °C |
0.142 BTU/lb-°F @Temperature 1470 °F |
|
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Specific Heat Capacity | 0.595 J/g-°C @Temperature 900 °C |
0.142 BTU/lb-°F @Temperature 1650 °F |
|
Haynes 556® alloy, bar, after 4000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |