Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 10 Polybutylene Terephthalate, 10% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 10% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B2 GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | STN EN 11357-1 |
Plastcom SLOVASTYR® B BT N PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Melting Point | 210 - 220 °C | 410 - 428 °F | ISO 11357-1 |
Radici Radilon® CST 38FL (dry) Copolyamide 6 semiaromatic Radilon® CS can be used for blown film extrusion in general as well as being particularly suited for co-extrusion with PE because it improves the transparency and thermoformability of the film.Appl.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B FRN 3 PBT, flame retarder FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 GF 10 MI PBT, 10% glass fibre Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B1 HML GF 10 PBT, 10% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 10% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Melting Point | 215 - 220 °C | 419 - 428 °F | Average value: 217 °C Grade Count:7 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | Average value: 219 °C Grade Count:6 |
Overview of materials for Nylon, Barrier Film Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Barrier Film Copolymer". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | crystalline melting point; Hot Stage Microscope |
Honeywell Capran® 512 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 512 LL is a heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other high temperature .. |
|||
Melting Point | 218 - 220 °C | 424 - 428 °F | crystalline melting point; Hot Stage Microscope |
Honeywell Capran® 980 Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 980 is a clear (low haze level), heat-stabilized cast film produced from modified nylon 6 resin. Capran® 980 has excellent heat stability and resistance to pinholing. It ca.. |
|||
Melting Point | 217 - 220 °C | 423 - 428 °F | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | |
Chase Plastics CP Pryme® N140MGHL (Dry) Nylon 6, 40% Glass Fiber Reinforced, Heat Stabilized, Lubricated Features: Heat StabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Melting Point | 216 - 220 °C | 420 - 428 °F | Average value: 220 °C Grade Count:24 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Melting Point | 200 - 220 °C | 392 - 428 °F | |
Plastcom SLOVASTER® B2 BT PBT, basic type FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of.. |