Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 10% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 30% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 40% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1293 - 1370 °C | 2359 - 2500 °F | |
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Melting Point | 1293 - 1370 °C | 2359 - 2500 °F | |
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Melting Point | 1300 - 1370 °C | 2370 - 2500 °F | |
Kennametal Stellite Denertiaâ„¢ N19 Nickel Dental Alloy Denertiaâ„¢ N19 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium freeInformation provided by Kennametal St.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Melting Point | 1293 - 1370 °C | 2359 - 2500 °F | |
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
HP Alloys Alloy C-276, 40% Cold Worked 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1334 - 1371 °C | 2433 - 2500 °F | |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness Tensile and bearing strengths (ultimate and yield) and elongation values reported here are typical for Cold Rolled Sheet, 3 Part Heat Treatment, 0.062 inch (1.57 mm) Thickness samples. Density and m.. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Bar Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special .. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Melting Point | 1324 - 1370 °C | 2415 - 2500 °F | |
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, GMAW deposit weld metal Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, plate, 1000 hours exposure at 760°C (1400°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Melting Point | 1325 - 1370 °C | 2417 - 2500 °F | |
HP Alloys Alloy C-276, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy plate, 8000 hours exposure at 649°C (1200°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Melting Point | 1301 - 1371 °C | 2374 - 2500 °F | |
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F) Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |