Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 312 °C | 594 °F | Peak; Dry; ASTM D3418 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melting Point | 312 °C | 594 °F | Dry; ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melting Point | 312 °C | 594 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Melting Point | 312 °C | 594 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Melting Point | 312 °C | 594 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |