Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 195 °C | 383 °F | ASTM D3418 |
Nylene® CX3451 Translucent Nylon Copolymer Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of.. |
|||
Melting Point | 195 °C | 383 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® V2603 Ethylene Vinyl Alcohol Copolymer Special designed the lowest ethylene content grade. Ethylene content 26 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
Melting Point | 195 - 205 °C | 383 - 401 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati.. |
|||
Melting Point | 195 - 198 °C | 383 - 388 °F | |
Hong Kun Group UV 360 UV Absorber UV360 areas of application include polyolefins (PP, PE), olefin copolymers such as EVA as well as blends of polypropylene with elastomers. In addition UV360 is highly effective in polyacetals, polya.. |
|||
Melting Point | 195 - 198 °C | 383 - 388 °F | |
Hong Kun Group UV 360 UV Absorber UV360 areas of application include polyolefins (PP, PE),olefin copolymers such as EVA as well as blends of polypropylene with elastomers. In addition UV360 is highly effective in polyacetals, polyam.. |
|||
Melting Point | 195 - 205 °C | 383 - 401 °F | |
UBE 7024B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Melting Point | 195 - 205 °C | 383 - 401 °F | |
UBE 7034B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Melting Point | 195 °C | 383 °F | ISO 3146 |
Chengdu Polyster FH2040 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H2040 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl.. |
|||
Melting Point | 195 °C | 383 °F | ISO 3146 |
Chengdu Polyster FH5550 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H5550 and self-made flame retardant material. Flame retardant, good balance of low and high temperature properties. Applications requiring flame retardancy, such as wires, cables and optica.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® XG5857 TPC-ET Extrusion Grade |
|||
Melting Point | 195 °C | 383 °F | |
Daikin NEOFLON RP-5000 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Melting Point | 195 °C | 383 °F | |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | ISO 11357 |
Arkema Group Pebax® MP 1878 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MP 1878 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. Added to PA6 Pebax® MP 1878 enhances the properties of PA6, especially at lo.. |
|||
Melting Point | 195 - 198 °C | 383 - 388 °F | ISO 3146 |
BASF Ultramid® C31 01 PA6/66 Description: Ultramid® C31 01 is a copolyamide 6/66 grade of low viscosity that is well suited for the production of compounds and blends. Product supplied in 2-2.5 mm CYLINDRICAL pellets.Informati.. |
|||
Melting Point | 195 °C | 383 °F | ISO 11357 |
Arkema Group Pebax® MP 1878 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MP 1878 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. Added to PA6 Pebax® MP 1878 enhances the properties of PA6, especially at lo.. |
|||
Melting Point | 195 - 225 °C | 383 - 437 °F | |
AIM 40In/60Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 195 - 197 °C | 383 - 387 °F | ISO 3146 |
BASF Ultramid® C33 PA6/66 Description: Ultramid® C33 is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film and monofilaments. Ultramid® C33 is well suited for the production of nonsymm.. |
|||
Melting Point | 195 - 215 °C | 383 - 419 °F | |
A. Schulman ComAlloy Hiloy® 640 Nylon 6/12, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 195 - 215 °C | 383 - 419 °F | |
A. Schulman ComAlloy Lubrilon® 646 Nylon 6/12, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® UM551 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |