Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 300TE BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 300TE BK602 is a medium-high viscosity toughened acetal homopolymer for injection molding with extremely low VOC emissions.Information provided by DuPont Performance Polymers |
|||
Melting Point | 178 - 186 °C | 352 - 367 °F | Average value: 178 °C Grade Count:17 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3024U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | 178 °C | 352 °F | ASTM D3418 |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20 EC PA12-CD25 Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process wit.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20 LM PA12 Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 20A Z PA12 Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-30H FWA nat PA12-GF30 Product description: Grilamid LV-30H FWA natural is a 30 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: Stiffness combined with h.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50 Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65 Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 3926 black 9992 PA12 Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 500T BK602 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T BK602 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the health.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® PC699 NC010 Acetal (POM)
(Unverified Data**) Lubricated Low Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for the Healthcare Industry Delrin SC699 is a low viscosity acetal homopolymer lubricated developed for parts req.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® LKN-3H PA12-GB30 Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Delrin® 300TE BK602 Acetal (POM)
(Unverified Data**) Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE BK602 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i.. |