Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
3M Dyneon™ PVDF 1012/0001 Polyvinylidene Fluoride
(discontinued **) High molecular weight grade PVDFSuitable for compression molding or extrusionExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent stre.. |
|||
Melting Point | 174 - 178 °C | 345 - 352 °F | Average value: 175 °C Grade Count:5 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
SK Chemicals SKYPEL G130D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | <= 174 °C | <= 345 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 02020 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 02020 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 02020 is an excellent sealing materi.. |
|||
Melting Point | <= 174 °C | <= 345 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 02020 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02020 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Dry) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AECV T8L Nylon 12, Cable Sheathing Grade (Conditioned) Designation ISO 1874-PA12,KHL,16-010Extrusion grade for the sheathing of wires and cables. Available colors: black, blue, orange and white. Reinforced light and heat stabilizing agents. Anti-termite.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent... |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | (Dry) |
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient.. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Melting Point | 174 °C | 345 °F | 10°C/min |
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
Ashley Polymers Ashlene® TD930H Nylon 12 A plasticized Nylon 12 offering outstanding flexibility with superior moisture and chemical resistance, UV and heat stabilized for weatherability.Data provided by the manufacturer |
|||
Melting Point | 174 °C | 345 °F | ASTM D3418 |
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Melting Point | 174 °C | 345 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |