Thermal Properties Metric English Comments
Melting Point 156 - 195 °C
313 - 383 °F
Average value: 176 °C Grade Count:31
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Melting Point 156 °C
313 °F
DSC
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
Melting Point 156 - 167 °C
313 - 333 °F
Huntsman/TMA
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically ..
Melting Point 156 - 161 °C
313 - 322 °F
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder
Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist..
Melting Point 156 - 165 °C
313 - 329 °F
10°C/min; ASTM D3418
Shanghai Ofluorine T-1 PVDF for coatings (DF-1)
Description: T-1 PVDF for coatings is solid powder, it can mixed with acrylic resin, additive, and become superior performance baking PVDF fluorocarbon coatings. Compared with other grade of PVDF, T..
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF)
Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The disper..
Melting Point 156 - 160 °C
313 - 320 °F
ISO 3146
Borealis Borflow™ HL508FB Polypropylene Homopolymer
Borflow HL508FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product ..
Melting Point 156 - 160 °C
313 - 320 °F
ISO 3146
Borealis Borflow™ HL512FB Polypropylene Homopolymer
Borflow HL512FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product ..
Melting Point 156 °C
313 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 50E571 Anhydride-Modified Polypropylene Adhesive Resin
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E561 and 50E571 are based on polypropylene random copolymers. They are available in pellet form for use in conventional ext..
Melting Point 156 °C
313 °F
ISO 3146
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE)
Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Melting Point <= 156 °C
<= 313 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Melting Point <= 156 °C
<= 313 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 15028EM1 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen..
Melting Point <= 156 °C
<= 313 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 40028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 40028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Melting Point <= 156 °C
<= 313 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Escorene™ UL 40028EM1 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen..
Melting Point 156 °C
313 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Elvamide® 8061 Nylon  (Unverified Data**)
Polyamide MultipolymerInformation provided by DuPont Performance Polymers
Melting Point 156 °C
313 °F
ASTM D3418
DuPont Performance Polymers Hytrel® G3548L TPC-ET  (Unverified Data**)
Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec..
Melting Point 156 - 160 °C
313 - 320 °F
ASTM D3418
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and ..
Melting Point 156 - 224 °C
313 - 435 °F
Average value: 203 °C Grade Count:93