Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FL 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FL 34 E is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 34 E is characterized by a good balance between processab.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3020 F LDPE Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3020 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3020 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3025 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3032 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3040 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
Hybrid Plastics POSS® MA0702 MethacrylIsobutyl-POSS® POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®.. |
|||
Melting Point | 114 °C | 237 °F | UBE method |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |
|||
Melting Point | 114 °C | 237 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 4033 Anhydride Modified HDPE BYNEL® Series 4000 resins are anhydride-modified, high-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process.. |
|||
Melting Point | 114 °C | 237 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Melting Point | 114 °C | 237 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® E528 Polymer Modifier DuPont™ Fusabond® E528 is a anhydride modified polyethylene. Used as a polymer modifier |
|||
Melting Point | 114 - 172 °C | 237 - 342 °F | Dow Method (DSC) |
Dow Saran® 506 Polymer Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity.. |
|||
Melting Point | 114 °C | 237 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Melting Point | 114 - 127 °C | 237 - 260 °F | Average value: 119 °C Grade Count:22 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Melting Point | 114 °C | 237 °F | ASTM D3418 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Melting Point | 114 °C | 237 °F | |
DuPont Fusabond® MB528D Linear Low Density Polyethylene
(discontinued **) Typical Use: Coupling agent for filled PE systems such as nonhalogen flame retardant filled wire and cable compoundsAdhesion promoterAvailability: North AmericaInformation provided by DuPont. |
|||
Melting Point | 114 °C | 237 °F | ISO 11357-3 |
Total Lacqtene® 1025 FH 24 LDPE blown film
(discontinued **) Radical polyethylene made by high pressure tubular process. Slip and antiblock formulated grade for good transparent thin films. Advised temperature profile : 150 to 190°C.Information provided prov.. |