Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 73.0 °C | 163 °F | Internal Method |
Polimeri Europa Greenflex® HN 70 Ethylene Vinyl Acetate Copolymer - Compounding Greenflex HN 70 is an ethylene vinyl acetate copolymer (EVA) for compounding applications. Greenflex HN 70 is a medium fluidity grade with high tack.Main Applications: Greenflex HN 70 is recommend.. |
|||
Melting Point | 73.0 °C | 163 °F | DSC |
Westlake EMAC® SP1400 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Melting Point | 73.0 - 77.0 °C | 163 - 171 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasti.. |
|||
Melting Point | 73.0 °C | 163 °F | Exxon Method |
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymer designed for specialty compounding applications. Excellent filler acceptance produces highly loaded concentrates.Ap.. |
|||
Melting Point | 73.0 °C | 163 °F | DSC |
Polyram BondyRam® 2001 Maleic Anhydride modified EVA coupling agent
(discontinued **) Maleic Anhydride Modified grafted EVA (28%VA) recommended as adhesive promoter and general purpose compatibilizerInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 73.0 °C | 163 °F | |
LG Chemical LC180 Polyolefin Elastomer Features: Excellent toughness with flexible performance, High clarity and low temperature sealability. High performance in footwear application.Application: Polymer modification, Shoe sole, Film coe.. |
|||
Melting Point | 73.0 - 93.0 °C | 163 - 199 °F | |
Indium Corp. Indalloy 35 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 73.0 - 77.0 °C | 163 - 171 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 508 Linear Thermoplastic Polyurethane Pearlbond™ 508 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules, with a high crystallization rate and a medium thermoplasticity level.Applica.. |
|||
Melting Point | 73.0 °C | 163 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3182 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 73.0 - 91.0 °C | 163 - 196 °F | ASTM D3418(DSC) |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melting Point | 72.8 °C | 163 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Escorene® LD 761.36 Molding, extrusion and compounding resin Escorene Ultra LD 761.36 is a 26.7% vinyl acetate copolymer excellent flexibility and low temperature toughness. LD 761.36 has high filler acceptance.Availability: Latin America, North America and S.. |
|||
Melting Point | 73.0 °C | 163 °F | ASTM D3418, ISO 3146 |
DuPont™ HPF® 2000 Amorphous Polymer for Golf Balls DuPont™ HPF 2000 offers high COR and lower compression. This combination of properties makes it extremely versatile and possible for this polymer to be used as a core, mantle, or cover in a golf ba.. |
|||
Melting Point | 73.0 °C | 163 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a.. |
|||
Melting Point | 73.0 °C | 163 °F | DSC |
Arkema Group LOTRYL® 37 EH 175 Copolymer Ethylene - 2-Ethylhexyl Acrylate LOTRYL® 37EH175 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. LOTRYL® 37EH175 is particularly recommended for the formulation o.. |
|||
Melting Point | 73.0 °C | 163 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 73.0 °C | 163 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |