Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 160 - 302 °C
320 - 576 °F
Average value: 295 °C Grade Count:20
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Melting Point 275 - 302 °C
527 - 576 °F
Indium Corp. Indalloy 242 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 275 - 302 °C
527 - 576 °F
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy
High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation.
Melting Point 275 - 302 °C
527 - 576 °F
Williams Advanced Alloys WS302 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys