Thermal Properties Metric English Comments
Melting Point 283 - 285 °C
541 - 545 °F
Average value: 284 °C Grade Count:6
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Melting Point 283 - 285 °C
541 - 545 °F
Average value: 284 °C Grade Count:13
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Melting Point 280 - 285 °C
536 - 545 °F
Average value: 281 °C Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Melting Point 239 - 285 °C
462 - 545 °F
Indium Corp. Indalloy 152 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 275 - 285 °C
527 - 545 °F
Solvay RHODAPHOSE® BINAP (RACEMIC) Phosphorus Derivative
Identification: 2,2’-BIS(DIPHENYLPHOSPHINO)-1,1’-BINAPHTHYLCAS: 98327 – 87 – 8Available in: Asia Pacific, Europe, Latin America and North America Applications: BINAP (RACEMIC) is a bulky phosphi..
Melting Point 280 - 285 °C
536 - 545 °F
Average value: 282 °C Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Melting Point 278 - 285 °C
532 - 545 °F
Average value: 282 °C Grade Count:29
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Copyright © lookpolymers.com All Rights Reserved