Thermal Properties Metric English Comments
Melting Point 182 - 187 °C
360 - 369 °F
Average value: 184 °C Grade Count:8
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Melting Point 183 - 187 °C
361 - 369 °F
Hong Kun Group AO 168 Antioxidant
CAS No. 31570-04-4All information provided by Hongkun Group
Melting Point 175 - 187 °C
347 - 369 °F
Huntsman/TMA
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
Melting Point 181 - 187 °C
358 - 369 °F
Indium Corp. Indalloy 226 Tin Solder Alloy
Zinc causes high dross U.S. Patent #5,242,658; covers 72.8-89.4Sn 6.7-19.2Zn 2.7-16.4In; temp. range Liq.. 176-193, Sol. 166-191.4Information Provided by Indium Corporation
Melting Point 175 - 187 °C
347 - 369 °F
Indium Corp. Indalloy® 227 Sn-In-Ag Solder Alloy
Pb free solder can be used as a replacement for 63Sn 37Pb, 62Sn 36Pb 2Ag and 60Sn 40Pb in that it has similar physical and mechanical properties. Not for use over 100°C due to 118°C Sn/In eut..
Melting Point 183 - 187 °C
361 - 369 °F
Suqian Unitechem Antioxidant 168
Chemical Name: Tris-(2,4-di-tert-butyl-phenyl)-phosphiteCAS NO.: 31570-04-4Molecular Formula: C42H63O3PProperties: The product takes on an appearance of white powder, without odor and smell. Solubl..
Melting Point 175 - 187 °C
347 - 369 °F
Williams Advanced Alloys WS187 Solder